Silicone injection molding follows different design rules than thermoplastic molding. Liquid silicone rubber (LSR) fills walls as thin as 0.25 mm, produces almost no sink marks, needs far less draft — but it flashes through gaps as small as 0.005 mm and shrinks 2.5–4.0% after curing. This guide gives the specific numbers to design against before you commit to tooling.

Quick Reference: LSR Design Specifications

ParameterDesign guideline
Minimum wall thickness0.25 mm (0.010 in) small areas · 0.38 mm (0.015 in) larger areas
Rib thickness0.5–1.0× adjoining wall
Wall thickness variationWell tolerated — sink marks almost nonexistent
Linear shrinkage2.5–4.0%
Post-cure shrinkage+0.5–0.7%
Flash thresholdFlashes in gaps ≥ 0.005 mm (0.0002 in)
Tolerance standardISO 3302-1, classes M1–M4
Draft angleMinimal required — material flexes on demold
Ejection methodManual or air-assisted — ejector pins normally not used
Insert bondingMechanical interlock — LSR does not chemically bond
Cure time in mold25–50 seconds

Why LSR Design Rules Differ from Thermoplastics

If you design silicone parts using injection molding habits carried over from thermoplastics, you will over-engineer some features and under-engineer others. Three fundamental differences drive every rule in this guide:

  • Thermoset, not thermoplastic. LSR is chilled before injection into a heated mold, where it cures permanently. Thermoplastic runs the opposite way — melted resin into a cooled mold. Once cured, silicone cannot be re-melted or reground.
  • Very low viscosity. LSR flows into features thermoplastics cannot fill — and into any gap in the tool, which is why flash control dominates tool design.
  • The finished part is elastic. A cured silicone part deforms to release from the tool, which relaxes draft and undercut constraints that would be hard limits in rigid plastic.

For a process-level comparison of LSR against solid silicone and how that affects tooling cost, see our guide to LSR vs HCR silicone.

Wall Thickness and Ribs

LSR fills thin sections readily. Published design guidance from on-demand manufacturer Protolabs puts achievable walls at 0.010 in (0.25 mm) in small areas, with 0.012 in (0.30 mm) practical over smaller spans and 0.015 in (0.38 mm) the safer figure over larger areas — the achievable minimum depends on the span of the thin wall and how close it sits to thicker sections (Protolabs, Designing for Liquid Silicone Rubber).

Rib thickness should be 0.5 to 1.0 times the adjoining wall thickness.

The advantage thermoplastic designers underuse

LSR tolerates wall thickness variation, and sink marks are almost nonexistent. In thermoplastic design, uniform wall thickness is close to sacred because thick sections sink and warp. In LSR you have real freedom to vary wall thickness for functional reasons — thicker sealing beads next to thin flexible membranes in the same part. Use it.

That said, thickness still has consequences: thick sections take longer to cure through, extending cycle time and unit cost, and wall thickness affects shrinkage behavior — thick walls shrink less than thin walls.

Shrinkage and Tolerance Strategy

Shrinkage is the single most common cause of failed first-article parts. Silicone is a thermoset that shrinks as it cools out of the heated mold.

  • LSR linear shrinkage: 2.5–4.0%
  • Additional shrinkage after oven post-cure: 0.5–0.7%

The mold must be cut oversize to compensate:

Cavity dimension = Target part dimension ÷ (1 − shrinkage rate)

Worked example: a seal with a 50.00 mm target outside diameter, in a compound with 2.8% expected shrinkage, requires a cavity of 50.00 ÷ (1 − 0.028) = 51.44 mm.

Tolerances follow ISO 3302-1, which defines four classes for molded rubber: M1 (precision), M2 (high quality), M3 (good quality) and M4 (non-critical), and distinguishes fixed dimensions from closure dimensions (ISO 3302-1:2014).

Tolerance strategy that controls cost
  1. Do not apply M1 across the whole drawing. Assign M1 only to sealing and mating surfaces; allow M3 on cosmetic and non-functional dimensions. Blanket precision tolerancing is the fastest way to inflate a tooling quote.
  2. Confirm the exact compound before cutting a precision tool. Shrinkage varies with filler loading, hardness, cure temperature and demold temperature — a generic 2.8% assumption is not a design basis.
  3. Compensate by zone. Shrinkage runs higher along the flow direction than perpendicular to it.
  4. Design steel-safe. Leave metal on the tool so cavities can be opened up after T0 trials rather than scrapped.
  5. Measure after post-cure, not straight out of the mold.

Draft, Ejection and Demolding

Rigid thermoplastic parts typically need meaningful draft to release. LSR needs far less, because the cured part is elastic and deforms as it comes off the core. Draft still helps — it shortens demold time and reduces tearing risk — but it is rarely the hard constraint it is in rigid plastic.

The more important consequence is how parts come out of the tool:

  • Ejector pins are normally not used in LSR molding, because the material's flash tendency means pin clearances become flash paths.
  • Parts are demolded manually, often with air assistance.
  • Design the part to stay on one half of the tool when the mold opens. If it is unpredictable which side the part stays on, cycle time and scrap both rise.

Radii: Where Silicone Parts Tear

LSR tears fairly easily at sharp edges. This is the failure mode that surprises designers coming from rigid plastics, where a sharp internal corner is a stress-concentration concern but rarely an immediate tear risk.

Add fillets and radii to internal features — particularly anywhere the part will be stretched during manual demolding, and anywhere an undercut must be pulled off a core by hand. A sharp internal corner at an undercut is a tear waiting to happen on the production floor, not just in service.

Remember: hardness does not equal tear resistance

Do not assume a harder compound resists tearing better. Published grade data shows Dow SE 1643 U at 31 Shore A delivers 48 N/mm tear strength — three times the 16 N/mm of DY 32-542 U at 42 Shore A. If your part has thin sections, undercuts or sharp internal geometry, specify a high-tear grade rather than simply raising durometer.

Parting Lines and Flash Control

LSR's low viscosity means it flashes through gaps as small as 0.0002 in (about 0.005 mm). For scale, that is well below the thickness of a human hair. Any tool gap that is not tightly controlled becomes a flash path.

Design implications:

  • Simplify and minimize parting lines. Fewer, simpler parting lines produce cleaner parts with less deflashing labor — which is unit cost, every part, forever.
  • Place parting lines on sharp edges or hidden surfaces, never across a sealing face or a cosmetic A-surface.
  • Define your flash spec on the drawing. Acceptable flash is a specification, not an assumption. State it explicitly, especially for food-contact and medical parts where flash is a cleaning and particulate concern.
  • Budget for deflashing if the geometry demands complex parting lines. Cryogenic deflashing is possible but adds a secondary operation.

Gates, Venting and Cold Runners

Gate placement determines where shrinkage concentrates and where cosmetic marks land.

  • Keep gates away from critical sealing and measurement surfaces. The gate vestige is a cosmetic and functional defect wherever it lands.
  • Shrinkage is directional — higher along the flow path than across it — so gate position directly changes which dimensions move most.
  • Venting matters more than in thermoplastics. Low-viscosity material traps air readily; inadequate venting shows up as short shots and voids.
  • Cold runner systems eliminate runner waste by keeping material uncured up to the gate. They add tooling cost but pay back in material savings at volume — worth evaluating during the DFM review rather than after.

Undercuts

Undercuts that would require side actions in rigid plastic can often be molded directly in LSR and stripped off the tool, because the cured part flexes. This is a genuine cost advantage — it can eliminate slides and lifters from the tool.

Two conditions apply:

  1. Radius every edge the part must stretch over. Sharp geometry plus manual stripping equals tearing.
  2. Verify with a prototype tool. Whether a specific undercut strips reliably at production speed depends on depth, durometer, tear strength and operator technique — confirm it before committing to a multi-cavity production tool.

Overmolding and Insert Molding

LSR is widely used to overmold plastic substrates and to insert-mold around metal components — soft-touch grips, sealed electronic housings, valve assemblies with metal inserts.

The rule that causes most overmolding failures

LSR generally does not chemically bond to substrates. Design mechanical interlocking features — throughholes, undercuts, grooves, knurling — into the substrate. Relying on adhesion alone is the most common cause of delamination in silicone overmolded assemblies.

Also verify substrate heat resistance. LSR cures in a hot mold, so the substrate must survive the cure temperature without distorting. High-temperature engineering plastics such as PEI, PEEK and PBT are commonly specified for this reason; commodity plastics frequently are not viable. Metal inserts must be dimensionally stable and clean — surface contamination is a bond failure mode, and platinum-cured LSR is sensitive to cure inhibition from certain contaminants including sulfur, amines and tin compounds.

Seven Design Mistakes That Cost Tooling Money

Common LSR design errors and their consequences
MistakeConsequence
Cutting the tool before the compound is confirmedShrinkage compensation is wrong; cavity is scrap or needs rework
Blanket M1 tolerances across the drawingTooling cost inflates with no functional benefit
Sharp internal corners at undercutsParts tear during demolding; scrap rate rises in production
Parting line across a sealing faceFlash on the sealing surface; leak failures in service
Gate on a critical or cosmetic surfaceVestige marks and localized dimensional deviation
Specifying durometer instead of tear strengthPart meets the spec on paper and fails in use
Overmolding without mechanical interlocksDelamination — silicone does not chemically bond

Pre-Tooling DFM Checklist

Work through these before steel is cut:

  • Exact silicone compound selected and its published shrinkage confirmed
  • Durometer and tear strength specified — not durometer alone
  • Minimum wall thickness verified against span and adjacent thick sections
  • Rib thickness set at 0.5–1.0× adjoining wall
  • Tolerance class assigned per dimension (M1 only where function requires it)
  • Shrinkage compensation calculated per zone, with steel-safe allowance
  • Parting line positioned off all sealing and cosmetic surfaces
  • Acceptable flash level stated on the drawing
  • Gate location confirmed away from critical dimensions
  • Fillets added at every internal corner and undercut edge
  • Part designed to remain on one mold half at opening
  • Mechanical interlocks designed into any overmold substrate
  • Substrate and insert materials verified for cure-temperature resistance
  • Post-cure requirement determined (cure system and compliance route)
  • Critical dimensions defined for measurement after post-cure

FAQ

What is the minimum wall thickness for LSR injection molding?

Walls as thin as 0.010 in (0.25 mm) are achievable over small areas, with roughly 0.015 in (0.38 mm) a safer minimum over larger spans. The achievable figure depends on the span of the thin section and its proximity to thicker regions.

How much draft angle does silicone injection molding need?

Far less than rigid thermoplastics. Cured silicone is elastic and deforms during demolding, so parts often release with minimal draft. Draft still helps reduce demold time and tearing risk, but it is rarely the limiting design constraint.

Why does my silicone part have flash?

LSR has very low viscosity and flashes through gaps as small as 0.0002 in (0.005 mm). Flash is controlled through tool design, clamp force, and parting line placement. Complex parting lines increase deflashing labor, so simplify them wherever possible.

Can LSR parts have undercuts?

Yes. Because cured silicone flexes, undercuts can often be stripped from the tool without side actions — frequently eliminating slides and reducing tooling cost. Add radii at all undercut edges to prevent tearing, and validate with a prototype tool first.

Does silicone bond to plastic in overmolding?

Generally not chemically. Design mechanical interlocking features such as throughholes, grooves or undercuts into the substrate. The substrate must also withstand LSR cure temperatures, which is why high-temperature plastics like PEI, PEEK and PBT are commonly specified.

What tolerances can silicone injection molding hold?

Molded rubber tolerances follow ISO 3302-1 classes M1 through M4. Precision class M1 is achievable on controlled dimensions with proper tooling and material characterization, but applying it across an entire part unnecessarily increases tooling cost.

Get a DFM Review Before You Cut Steel

SILICONE SOLUTION is a China-based custom silicone manufacturer in Xiamen, exporting to 55+ countries, with ISO 9001 and ISO 13485 certified production and ISO 8 cleanroom capability. We run LSR injection, compression, transfer and extrusion lines in-house, backed by our own precision mold shop — so tooling revisions happen under one roof.

Send your drawing or 3D file and our engineers will review wall thickness, shrinkage compensation, parting line and gate strategy, and tolerance assignment against your functional requirements. Quotations within 24 hours, prototypes in about 7 days.

Request a DFM Review →

References

  1. Protolabs — Designing Liquid Silicone Rubber Prototypes and Components (wall thickness, rib ratio, flash threshold, ejection and undercut guidance).
  2. Holtz, T., Protolabs, in Medical Design & Outsourcing — How to design liquid silicone rubber prototypes and components.
  3. ISO 3302-1:2014 — Rubber: Tolerances for products, Part 1: Dimensional tolerances.
  4. ASTM D2240 (hardness), ASTM D624 (tear strength).
  5. Published manufacturer datasheets: Dow DY 32-542 U, Dow SE 1643 U.

Enrique

Hi, I am the author of this article. For the past 10 years or so, we have been dedicated to meeting the custom silicone product needs of our customers from over 50 countries and regions around the world. If you have any questions, please contact us for a free, no-obligation quote.

Share this article now

Leave A Comment

Looking for a Reliable and Efficient Silicone Manufacturer?

Partner with SILICONE SOLUTION for top-quality manufacturing services. Contact us today to discuss your specific needs and discover how we can help bring your vision to life!

Please fill out our form and our silicone experts will contact you within 24 hours.